RedLine 0 Posted October 7, 2010 Share Posted October 7, 2010 Hi 5/6mm thin vertical bulkheads that take the weight of the cockpit floor down to the hull on my 930 have gone mushy, and started to de-laminate, with some parts coming away from the hull tabs. Am intending on drying them out, peeling/cutting away any delaminated areas, and glassing both sides from under cockpit floor, over the bulkheads, and down onto the tabs on the hull. This will seal the wood, and give put some strength back. What would be the best weight of cloth to use. Local Burnsco only has 200g woven cloth. Would this be ok, and if so how many layers to use 1/2/ 3? Dont want to use CSM as its messy to work with. Any advice appreciated Link to post Share on other sites