Galvanic Corrosion on Boom

Recommended Posts

These little lugs (x4) under the boom for the lazy jacks were installed about 4 years ago. I've noticed not insignificant equal corrosion at all four points.

 

There are several other stainless fixtures on the mast and boom that have existed longer and don't show any where near the same amount of corrosion.

 

There is no corrosion inside the boom.

 

I can't tell if the rivets are stainless or aluminium. I have drilled them off and will reattach them with aluminium rivets and will put an insulating washer between them.

 

But the stainless will still be 'connected' via the rivet. So will just the rivet corrode or will the boom continue to corrode through the rivet? And therefore do I need to completely insulate the stainless?

 

(I guess plastic rivets are a thing?)

Screenshot_20191231-111035_Gallery.jpg

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.
Note: Your post will require moderator approval before it will be visible.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Loading...
Sign in to follow this  

×
×
  • Create New...